Special Processing: EDM
?
Electric spark machining (EDM) is a process for machining extremely hard and exotic materials such as graphite, superalloys, and stainless steel. It is also used to produce high-precision parts with tight tolerances, complex geometries, very low surface roughness, and minimal burr.
EDM involves......