Niobium in future consumption
Introduction
Niobium, a transition metal with symbol Nb and atomic number 41, is a hard, grey, silvery crystalline element. Niobium offers a combination of properties, such as strength, low electrical resistivity, and low thermal expansion, which have made it an important material in a variety of......